Colors

TPU98A is available from stock in 6 colors.
For other non stock colors please ask our team.

Standard

CL1 Clear
BK1 Black
WH1 White
RD1 Red
BU2 Dark Blue
PI2 Soft Pink

TPU98A

TPU98A is a specifically formulated flexible filament for easy & high speed printing on both direct and Bowden style 3D printers. TPU98A features an exceptionally high heat resistance (138℃) and can be stretched as far as 450% before reaching its breaking point. TPU98A does not require the use of a heated bed and can even be printed straight onto (clean) glass. TPU98A is the flexible filament for (semi)professional users who do not want to compromise and require a high mechanical flexible filament that prints easily. TPU98A is an extremely usable flex-filament with a wide variety of different applications such as Orthopedic insoles, Prosthetics, Vibration dampers and many more.

Features:

  • Strong & Flexible
  • Works on Direct & Bowden style 3D printers
  • Printable at speeds of >75mm/s
  • Exceptionally high softening point of 138℃
  • 450% elongation at break
  • Resistance to oils, greases
  • Easily printed water-tight
Size ø Tolerance Roundness
1,75mm ø 0,05mm 95%
2,85mm ø 0,10mm 95%
Description Test method Typical value
Specific gravity ISO 1183 1,16 g/cc
Tensile strength at yield ISO 1133 57 g/10min
Tensile strength at yield ISO 527 50 MPa
Elongation strain at break ISO 527 450%
Tensile (E) modulus ISO 527 150 MPa
Impact strength - Charpy method 23˚C ISO 179 1eA N.B.
Shore hardness ISO 7619-1 98A
Melting temp. ISO 294 225°C
Glass transition (Tg) ISO 11357 -16°C
Vicat softening temp. ISO 306 138°C
Description Test method Typical value
printing temp. Internal method 230±10˚C

Packaging

TPU98A is available in nearly any type of packaging and labelling. Ask our team to help you customizing your product.

Additional information

TPU98A does not require a heated bed to stick well though you can set it to ≤60°C for extra reassurance.
TPU98A works superb with a direct drive feeder, or newer types of Bowden FDM or FFF technology 3D printers.
By changing the infill / amount of walls you can create the perception of a higher / lower shore than 98A.

Storage

Cool and dry (15-25˚C) and away from UV light. This enhances the shelf life significantly.

We will supply this product with a moisture content <0,2%. After being out of the bag for several hours, redrying in an oven is recommended to eliminate moisture. See page 4 for the recommended drying time and temperatures.

Downloads